Low Melt Fusible Alloy 95

For Lost-Core Mandrels & Workholding

LM95 is a premium, cadmium-free low-melting-point alloy formulated specifically for its precise eutectic melting point and expansion properties. It transitions cleanly from liquid to solid with zero mushy range.

The alloy initialises with a volumetric contraction for effortless tool release, followed by a controlled solid growth to tightly grip composite plies or lock delicate workpieces securely in place. It is the dependable choice for technicians requiring flawless surface replication and easy, melt-out reclamation.

Lost-Core Mandrels

Cast highly intricate, seamless solid mandrels for hollow composite layups. The alloy handles curing pressures easily, then cleanly melts out in a hot water bath above 95°C for 100% material reclamation.

Precision Workholding

Safely encapsulate delicate, thin-walled, or irregular components for machining or grinding. The +0.61% solid growth ensures a zero-slip mechanical grip that leaves no distortion when melted away.

Thermal Safety Links

Utilise the sharp, predictable 95°C eutectic transition point for safety-critical thermal triggers, environmental release mechanisms, and low-temperature fire protection triggers.

Product Specifications

Property Value
Composition Bi52.5, Pb32.0, Sn15.5
Liquidus 95°C (203°F)
Solidus 95°C (203°F)
Density 9.71 g/cm³
Brinell Hardness 9
Volume Change
(Liquid to Solid)
-1.5% (Shrinkage)
Tensile Strength 19.0 MPa
Solid Growth +0.55% linear growth (1 hour)
+0.57% linear growth (24 hours)
+0.61% linear growth (500 hours)

Product Sizing & Form Availability

  • Standard 1kg Bars: The industry-go-to format for easy workshop handling, precise pot loading, and rapid, efficient melting. Neatly packed into 25kg boxes.
  • Bespoke Manufacturing: Custom sizing available, contact our sales team with your requirements and we can try our best to accommodate!

Working with equipment calibrated in Fahrenheit? Convert here using our conversion tool:

Frequently Asked Questions

What is the exact melting point of LM95, and how do I melt it out?+
How does LM95 shrink and expand after casting?+
Is LM95 cadmium-free, and what is its alloy composition?+
Can LM95 be reclaimed and reused after melting out?+

Product Enquiry